https://www.selleckchem.com/pr....oducts/Vorinostat-sa
The 224 nm sample with the minimum values oft,s, and Cr-O1-Cr bond angle exhibits the maximum value of MEC (-ΔS) = 37.8 J kg-1 K-1at 5 K under a field variation (ΔH) of 7 T and its large estimated RCP of 623.6 J Kg-1is comparable with those of typical MC materials. Both (-ΔS) and RCP are shown to scale with the saturation magnetizationMS, suggesting thatMSis the crucial factor controlling their magnitudes. Assuming (-ΔS) ∼ (ΔH)n, the temperature dependence ofnfor the six samples are determined,nvarying between 1.3 at 5 K ton= 2.