https://bbi608inhibitor.com/an....-infrequent-case-of-
The 047-14 m range reveals transparency, a suitable bandgap, and a lower melting point in comparison to LiGaSe2 and LiInSe2. A more technologically sophisticated growth process is facilitated by the wider homogeneity range in the phase diagram's representation. Employing the two-zone temperature method, we produced the LiGa05In05Se2 polycrystal in this work. Employing a modified Bridgman method, 26 mm x 50 mm LiGa05In05Se2 single crystals