Two types of dense and toughened 3Y-TZP zirconia implants were fabricated by the sintering of green compacts. Then, the sintered properties of the two implants were compared. Slip-cast and post-sintered all-ceramic zirconia implants were fabricated by the heat treatment at 1450 °C for 2 h using optimal slurry conditions (60 wt% solid content, 1 wt% dispersant, and pH 12). Computer-aided design and manufacturing (CAD/CAM)-machined and post-sintered zirconia crowns, supplied by a dental hospital, were obtained by sintering at 1650 °C for 5